Sphelite ACD-800A Gallium Extraction Chelating Resin 0.3-0.6mm Macroporous Beads
Product Details:
| Place of Origin: | China |
| Brand Name: | ADVSORBENT |
| Certification: | ISO 9001:2015 |
| Model Number: | ACD-800A |
Payment & Shipping Terms:
| Minimum Order Quantity: | 25 Liters |
|---|---|
| Price: | USD 30-60 / Liter |
| Packaging Details: | 25 liters/bag, 50 liters/drum (dry type), 200 liters/drum, 1 ton pallet, or customized |
| Delivery Time: | 7-15 working days after order confirmation |
| Payment Terms: | T/T, L/C, Western Union, PayPal |
| Supply Ability: | 1000 Tons per Year |
|
Detail Information |
|||
| Structure: | Styrene-Acrylonitrile Copolymer | Appearance: | White To Pale Yellow Opaque Spherical Beads |
|---|---|---|---|
| Particle Size Range: | 0.3-0.6 Mm (95% Minimum) | Shipping Weight: | 0.72-0.82 G/ml |
| Moisture Content: | 45-55% | Sphericity After Attrition: | 90% Minimum |
| Gallium Adsorption Capacity: | 15 G/L Minimum | Application: | Selective Gallium Extraction From Bayer Process Alumina Mother Liquor |
| Highlight: | Gallium Extraction Chelating Resin,Macroporous Chelating Resin Beads,0.3-0.6mm Chelating Resin |
||
Product Description
Product Introduction
Sphelite ACD-800A is a macroporous chelating resin built on a styrene-acrylonitrile copolymer matrix. Special functional groups with high affinity and selectivity for gallium ions (Ga3+) are grafted onto the polymer backbone. Its working mechanism relies mainly on coordination chemistry (chelation) rather than simple ion exchange, enabling low-cost, low-energy and high-efficiency selective enrichment of gallium from Bayer-process alumina mother liquor.
Technical Indexes
| Appearance | White to pale yellow opaque spherical beads |
| Structure | Styrene-Acrylonitrile Copolymer |
| Particle Size Range (mm) | ≥ 95% 0.3-0.6 |
| Shipping Weight (g/ml) | 0.72-0.82 |
| Moisture Content (%) | 45-55 |
| Sphericity after Attrition (%) | ≥ 90 |
| Gallium Adsorption Capacity (g/L) | ≥ 15 |
Key Applications
- Selective recovery of gallium metal ions from Bayer-process alumina mother liquor.
- Hydrometallurgical enrichment and purification of gallium (Ga) resources.
- Low-cost, low-energy alternative to solvent extraction for gallium recovery.
Operating Conditions
Pre-treatment: Rinse resin with 1-2BV pure water.
Adsorption Conditions: Suspended solids (SS) ≤ 1 ppm.
Regeneration:
- Regenerants: 4-6BV 5% H2SO4 and 2BV 5.0 mol/L NaOH
- Concentration: 5% H2SO4, 5.0 mol/L NaOH
- Flow rates: 1-1.5BV/h (H2SO4), 2BV/h (water & NaOH)
- Rinse resin with 2-4BV pure water after acid elution prior to NaOH activation
Storage
Storage temperature shall not exceed 90°C; store above 0°C in wet state. Keep the package sealed to prevent water loss. If the resin dries out, soak it in ethanol for about 2 hours, wash with clean water, then repackage or use. Prevent the beads from freezing and cracking in winter; if frozen, melt slowly at room temperature.
Packaging
25 liters/bag · >25KG/bag · 50 liters/drum (dry type) · >200 liters/drum · >1 cbm on a pallet · 1 Ton on a pallet. Customized packaging is available to meet domestic and international transportation standards.